# Dalian HuntHumber Plastic Co., Ltd. (HuntHumber) > Specialist manufacturer (est. 2007, Dalian, China) of maleic anhydride (MAH) grafted polyolefin adhesive resins, tie layers, coupling agents, and compatibilizers based on EVA, LDPE, LLDPE, POE, and PP. Certified to ISO 9001 & ISO 14001 (SGS). Catalog baseline: catalog-2026-09-19-mfr-corrected (22 core grades) Full machine-readable specification table: https://www.hunthumber.com/llms-full.txt ## Core Sections - [Product Grade Selector](https://www.hunthumber.com/products/): Filter MAH-g-PO adhesive resin and compatibilizer grades by family, base resin, MAH band, and substrate. - [Applications](https://www.hunthumber.com/applications/): Panel bonding (ACP), multilayer EVOH/PA barrier packaging & pipes, HFFR cables, PA toughening, and WPC. - [Document Center (TDS, SDS, RDS)](https://www.hunthumber.com/portal/): Registered customer download center for Technical Data Sheets (TDS), Safety Data Sheets (SDS / MSDS), and Regulatory Data Sheets (RDS). - [Technical Notes](https://www.hunthumber.com/resources/): Engineering notes and primary research references. - [About & Certifications](https://www.hunthumber.com/about/): Dalian manufacturing plant, QC laboratory, SGS ISO 9001/14001, RoHS, REACH, grade-specific food-contact support, and invention patents. - [Contact & Sample Request](https://www.hunthumber.com/contact/): enquiry@hunthumber.com (unified domestic & international sales and technical desk). - [Chinese Version](https://www.hunthumber.com/zh/): Simplified Chinese mirror of the product catalog and engineering guides. ## Application Solutions - [Panel Bonding Resins (ACP & Metal-Polyolefin Laminates)](https://www.hunthumber.com/applications/panel-bonding/): MAH-grafted EVA, LDPE, and LLDPE tie resins engineered for aluminum, galvanized steel, stainless steel, PE core, and wood composite panels. - [Multilayer Coextruded Barrier Packaging & Oxygen-Barrier Pipe](https://www.hunthumber.com/applications/barrier-packaging/): LLDPE-based MAH-grafted tie layers delivering reliable interlayer adhesion between EVOH, PA (nylon), and PE across blown film, cast film, blow molding, and PEX/EVOH pipes. - [Coupling Agents & Compatibilizers for Compounding](https://www.hunthumber.com/applications/compounding/): High-reactivity MAH-grafted PE, POE, and PP modifiers for halogen-free flame-retardant (LSZH/HFFR) cables, low-temperature nylon toughening, and fiber-reinforced composites. ## Core Grades - [JME30A](https://www.hunthumber.com/products/jme30a/): EVA, Density 0.938 g/cm³, MFR 3.0 g/10 min, Tm 96 °C, MAH Low, Panel Bonding Resins (Al, SS, PE, Wood). - [JMV300](https://www.hunthumber.com/products/jmv300/): LLDPE, Density 0.930 g/cm³, MFR 2.8 g/10 min, Tm 125 °C, MAH Low, Panel Bonding Resins (Al, PE). - [JME30C](https://www.hunthumber.com/products/jme30c/): EVA, Density 0.935 g/cm³, MFR 3.0 g/10 min, Tm 98 °C, MAH Low, Panel Bonding Resins (Al, SS, PE, Wood). - [JMV240](https://www.hunthumber.com/products/jmv240/): EVA, Density 0.935 g/cm³, MFR 2.4 g/10 min, Tm 102 °C, MAH Low, Panel Bonding Resins (Al, GS, Wood, PE). - [LHT808](https://www.hunthumber.com/products/lht808/): EVA, Density 0.928 g/cm³, MFR 2.3 g/10 min, Tm 96 °C, MAH Low, Panel Bonding Resins (Al). - [JMV400](https://www.hunthumber.com/products/jmv400/): LLDPE, Density 0.930 g/cm³, MFR 4.1 g/10 min, Tm 125 °C, MAH Low, Panel Bonding Resins (Al, GS, PE). - [JMV260](https://www.hunthumber.com/products/jmv260/): LDPE, Density 0.935 g/cm³, MFR 2.8 g/10 min, Tm 105 °C, MAH Low, Panel Bonding Resins (Al, GS, PE). - [JMV265](https://www.hunthumber.com/products/jmv265/): LDPE, Density 0.930 g/cm³, MFR 2.3 g/10 min, Tm 115 °C, MAH Low, Panel Bonding Resins (Al, GS, PE). - [AT3016](https://www.hunthumber.com/products/at3016/): LLDPE, Density 0.920 g/cm³, MFR 2.0 g/10 min, Tm 121 °C, MAH Low, Multilayer Barrier Packaging (PA, PE). - [AT3018](https://www.hunthumber.com/products/at3018/): LLDPE, Density 0.920 g/cm³, MFR 1.8 g/10 min, Tm 121 °C, MAH Medium, Multilayer Barrier Packaging (PA, PE). - [AT2718](https://www.hunthumber.com/products/at2718/): LLDPE, Density 0.918 g/cm³, MFR 2.7 g/10 min, Tm 115 °C, MAH High, Multilayer Barrier Packaging (PA, PE). - [AT2018](https://www.hunthumber.com/products/at2018/): LLDPE, Density 0.920 g/cm³, MFR 1.7 g/10 min, Tm 121 °C, MAH High, Multilayer Barrier Packaging (EVOH, PA, PE). - [AT45C](https://www.hunthumber.com/products/at45c/): LLDPE, Density 0.930 g/cm³, MFR 4.5 g/10 min, Tm 125 °C, MAH Low, Multilayer Barrier Packaging (PA, PE). - [AD318](https://www.hunthumber.com/products/ad318/): LLDPE, Density 0.915 g/cm³, MFR 1.9 g/10 min, Tm 119 °C, MAH Medium, Multilayer Barrier Packaging (EVOH, PA, PE). - [AD428](https://www.hunthumber.com/products/ad428/): LLDPE, Density 0.910 g/cm³, MFR 1.7 g/10 min, Tm 119 °C, MAH Medium, Multilayer Barrier Packaging (EVOH, PA, PE). - [AD1816](https://www.hunthumber.com/products/ad1816/): LLDPE, Density 0.924 g/cm³, MFR 2.2 g/10 min, Tm 121 °C, MAH Low, Multilayer Barrier Packaging (EVOH, PA, PE). - [CT1516](https://www.hunthumber.com/products/ct1516/): PE, Density 0.928 g/cm³, MFR 1.9 g/10 min, Tm 120 °C, MAH High, Coupling Agents & Compatibilizers (PE, mineral fillers). - [CT1216](https://www.hunthumber.com/products/ct1216/): LLDPE, Density 0.910 g/cm³, MFR 1.2 g/10 min, Tm 113 °C, MAH High, Coupling Agents & Compatibilizers (Mg(OH)2, Al(OH)3, mineral fillers). - [PGN20](https://www.hunthumber.com/products/pgn20/): POE, Density 0.872 g/cm³, MFR 1.8 g/10 min, Tm 52 °C, MAH Medium, Coupling Agents & Compatibilizers (PA). - [PGN4018](https://www.hunthumber.com/products/pgn4018/): POE, Density 0.875 g/cm³, MFR 1.2 g/10 min, Tm 58 °C, MAH High, Coupling Agents & Compatibilizers (PA). - [WPX500](https://www.hunthumber.com/products/wpx500/): LLDPE, Density 0.910 g/cm³, MFR n.a. g/10 min, Tm 102 °C, MAH Very High, Coupling Agents & Compatibilizers (Natural fibers). - [PX316](https://www.hunthumber.com/products/px316/): PP, Density 0.904 g/cm³, MFR 60 g/10 min, Tm 160 °C, MAH High, Coupling Agents & Compatibilizers (Glass fibers, Natural fibers). ## Engineering Guides - [Reading a peel test on an aluminium composite panel](https://www.hunthumber.com/resources/selecting-acp-bonding-resin/): Two panels can give the same peel force and fail in different layers. The force trace and the fracture surfaces belong in the same test record. - [When oxygen transmission rises in an EVOH laminate](https://www.hunthumber.com/resources/evoh-pa-pe-tie-layer-guide/): Humidity, local thinning and delamination call for different measurements. A single oxygen transmission rate cannot distinguish them. - [Where the mineral filler sits in an HFFR cable compound](https://www.hunthumber.com/resources/hffr-cable-pa-compatibilizer-guide/): Filler content alone does not describe an EVA/LLDPE compound. Its distribution between the two polymer phases can change the fracture surface and the tensile response. - [EVA-Based vs. PE-Based Adhesive Resins for Metal Lamination: Polymer Architecture, Thermal Processing Windows, and Selection Boundaries](https://www.hunthumber.com/resources/eva-vs-pe-adhesive-resins-metal-lamination/): A first-principles comparison of EVA-based and PE-based maleic anhydride-grafted adhesive resins in aluminium composite panel (ACP) lamination, covering crystallinity, polarity, thermal degradation limits, and core compatibility. - [Why Initial Peel Strength Does Not Guarantee Long-Term Durability: Hygrothermal Ageing, Thermal Cycling, and Interfacial Degradation Mechanisms](https://www.hunthumber.com/resources/why-initial-peel-strength-does-not-guarantee-durability/): Explains why high dry ambient peel strength can mask fragile physical adsorption, dissecting water-induced interfacial displacement, aluminium oxide hydration, CTE thermal fatigue, and post-crystallisation stress alongside an accelerated ageing verification matrix. - [Concentrated vs. Ready-to-Use Tie-Layer Resins: Mixing Dynamics, Interfacial Coverage, and Total Process Cost Analysis](https://www.hunthumber.com/resources/concentrated-vs-ready-to-use-tie-layer-resins/): Examines the engineering trade-offs between in-house dry-blending of functionalised tie concentrates and pre-compounded ready-to-use tie resins through single-screw mixing dynamics, viscosity ratios, ultra-thin layer coverage, and Total Cost of Ownership (TCO). - [How Aluminium Surface Treatment Affects Polymer Adhesion: Conversion Coating Chemistry, Wetting Behaviour, and Delamination Diagnostics](https://www.hunthumber.com/resources/aluminium-surface-treatment-polymer-adhesion/): Examines how rolling oils, native aluminium oxides, chromate vs. chrome-free conversion coatings, and back-coat primers govern covalent bonding with MAH-grafted tie resins, complete with a rapid 30-minute shop-floor diagnostic protocol. - [Understanding Adhesive Film Thickness in Composite Panels: Wetting Fill, Stress Buffering, and Thermal Transfer Balance](https://www.hunthumber.com/resources/understanding-adhesive-film-thickness-composite-panels/): Defines the lower and upper engineering boundaries of adhesive film thickness in aluminium composite panels (ACP), examining core micro-roughness filling, CTE shear-strain buffering, heat-transfer lag, and gauge-tolerance discipline. - [The Role of Cooling and Crystallisation in Thermoplastic Bonding: Residual Stress, Curling, and Post-Crystallisation Evolution](https://www.hunthumber.com/resources/cooling-and-crystallisation-in-thermoplastic-bonding/): Explains how cooling rate, semi-crystalline solidification shrinkage, and 24–72 hour post-crystallisation alter measured peel strength and flatness in multilayer films, pipes, and metal composite panels, with four cooling-zone engineering controls. - [Tie-Layer Performance in Retort Packaging: Interfacial Stability Under 121°C Hygrothermal Sterilisation](https://www.hunthumber.com/resources/tie-layer-performance-in-retort-packaging/): Analyses thermal softening, steam permeation, Retort Shock, thermoforming corner thinning, and hydrolytic attack in PP/Tie/EVOH/Tie/PP structures under 121°C retort sterilisation, outlining PP-based tie-resin selection and validation protocols. - [Understanding Interfacial Instability in Multilayer Coextrusion: Viscosity Ratios, Elasticity Mismatch, and Die-Channel Control](https://www.hunthumber.com/resources/interfacial-instability-in-multilayer-coextrusion/): Dissects viscous encapsulation, high-frequency zigzag instability, and low-frequency wave instability in multilayer barrier films and pipes, explaining why MFR alone misleads rheology matching and outlining shop-floor troubleshooting steps. - [Designing a Reliable Adhesive Resin Qualification Trial: Baselines, Sampling Matrices, and Release Criteria](https://www.hunthumber.com/resources/designing-reliable-adhesive-resin-qualification-trial/): A practical shop-floor SOP for qualifying alternative or new adhesive tie resins without false passes or false failures, covering control baselines, purge stabilisation, process-window stress testing, multi-point sampling, and post-ageing release criteria. - [Regrind and Recycled Materials in Multilayer Structures: Compatibilising EVOH/PA Streams and Controlling Gel Formation](https://www.hunthumber.com/resources/regrind-and-recycled-materials-in-multilayer-structures/): Examines phase morphology, over-crosslinking gel risks, moisture control, dedicated regrind-layer design, and measured compatibiliser dosing when reincorporating EVOH- and PA-containing multilayer scrap back into coextrusion lines.