Skip to main content
HuntHumber

TN-03 2 min read Compounding

Where the mineral filler sits in an HFFR cable compound

Filler content alone does not describe an EVA/LLDPE compound. Its distribution between the two polymer phases can change the fracture surface and the tensile response.

A change that calorimetry missed

Heinz and colleagues studied magnesium hydroxide in an equal-parts EVA/LLDPE blend. When they replaced part of the LLDPE with a grafted coupling agent, microscopy showed smaller polymer domains and a shift of filler from mainly the EVA phase towards the interphase. Differential scanning calorimetry showed no detectable coupling-agent effect in the same study.

Distinguish dispersion from location

A large aggregate and a well-dispersed particle in the wrong phase pose different questions. Inspect several fields at the same magnification. Look for clusters, particle pull-out and the size of the polymer domains. If contrast does not distinguish the two polymers, a fracture image alone cannot establish which phase contains the filler.

Keep the control formulation comparable

Keep mineral loading, particle treatment and mixing history fixed. Replace an equivalent mass of carrier when introducing a coupling agent so the mineral fraction stays constant. Compare tensile strength and elongation on specimens with the same conditioning. Where fire performance matters, record the relevant fire test separately. A tensile result cannot establish the fire classification of a finished cable.

Reference · M. Heinz et al., Halogen-free flame-retardant cable compounds: Influence of magnesium-di-hydroxide filler and coupling agent on EVA/LLDPE blend system morphology