TN-01 Panel Bonding 2 min read
Reading a peel test on an aluminium composite panel
Two panels can give the same peel force and fail in different layers. The force trace and the fracture surfaces belong in the same test record.
Engineering notes
How grafted polyolefin systems behave at the interface: wetting, crystallisation, ageing, and what a trial has to measure before a line changes over.
TN-01 Panel Bonding 2 min read
Two panels can give the same peel force and fail in different layers. The force trace and the fracture surfaces belong in the same test record.
4 notes
TN-08
5 min read
Defines the lower and upper engineering boundaries of adhesive film thickness in aluminium composite panels (ACP), examining core micro-roughness filling, CTE shear-strain buffering, heat-transfer lag, and gauge-tolerance discipline.
TN-07
6 min read
Examines how rolling oils, native aluminium oxides, chromate vs. chrome-free conversion coatings, and back-coat primers govern covalent bonding with MAH-grafted tie resins, complete with a rapid 30-minute shop-floor diagnostic protocol.
TN-04
6 min read
A first-principles comparison of EVA-based and PE-based maleic anhydride-grafted adhesive resins in aluminium composite panel (ACP) lamination, covering crystallinity, polarity, thermal degradation limits, and core compatibility.
5 notes
TN-13
6 min read
Examines phase morphology, over-crosslinking gel risks, moisture control, dedicated regrind-layer design, and measured compatibiliser dosing when reincorporating EVOH- and PA-containing multilayer scrap back into coextrusion lines.
TN-11
6 min read
Dissects viscous encapsulation, high-frequency zigzag instability, and low-frequency wave instability in multilayer barrier films and pipes, explaining why MFR alone misleads rheology matching and outlining shop-floor troubleshooting steps.
TN-10
6 min read
Analyses thermal softening, steam permeation, Retort Shock, thermoforming corner thinning, and hydrolytic attack in PP/Tie/EVOH/Tie/PP structures under 121°C retort sterilisation, outlining PP-based tie-resin selection and validation protocols.
TN-06
6 min read
Examines the engineering trade-offs between in-house dry-blending of functionalised tie concentrates and pre-compounded ready-to-use tie resins through single-screw mixing dynamics, viscosity ratios, ultra-thin layer coverage, and Total Cost of Ownership (TCO).
TN-02
2 min read
Humidity, local thinning and delamination call for different measurements. A single oxygen transmission rate cannot distinguish them.
3 notes
TN-12
6 min read
A practical shop-floor SOP for qualifying alternative or new adhesive tie resins without false passes or false failures, covering control baselines, purge stabilisation, process-window stress testing, multi-point sampling, and post-ageing release criteria.
TN-09
6 min read
Explains how cooling rate, semi-crystalline solidification shrinkage, and 24–72 hour post-crystallisation alter measured peel strength and flatness in multilayer films, pipes, and metal composite panels, with four cooling-zone engineering controls.
TN-05
6 min read
Explains why high dry ambient peel strength can mask fragile physical adsorption, dissecting water-induced interfacial displacement, aluminium oxide hydration, CTE thermal fatigue, and post-crystallisation stress alongside an accelerated ageing verification matrix.